Comparison of crack driving force estimation schemes for weld defects in reeled pipelines Breadcrumbs UL Home Research Publications Year of Publication 2007 Journal Proceedings Of The Seventeenth (2007) International Offshore And Polar Engineering Conference, Vol 1- 4, Proceedings